Alternate Names: Frit 404, Frit P404
Description: High temperature leadless boron free glaze flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 17.80% | 0.22 | |
| CaO | 12.20% | 0.41 | |
| K2O | 12.00% | 0.24 | |
| Na2O | 4.60% | 0.14 | |
| Al2O3 | 10.80% | 0.20 | |
| SiO2 | 42.60% | 1.32 | |
| Oxide Weight | 186.86 | ||
| Formula Weight | 186.86 | ||
| Materials |
Ferro Frit 3831
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 488
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 13.00 |
|---|---|
| Co-efficient of Linear Expansion | 13.0 x 10-6 (50-450C) |
| Frit Melting Range (C) | 1430-1960F |