Alternate Names: Frit 318, Frit P318
Description: Leadless high barium zero alumina borosilicate flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 41.90% | 1.00 | |
| B2O3 | 19.90% | 1.05 | |
| SiO2 | 38.20% | 2.33 | |
| Oxide Weight | 365.87 | ||
| Formula Weight | 365.87 | ||
Used in partially-fritted matte and art glazes.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 385
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.0 x 10-6 (50-450C) |
|---|---|
| Frit Melting Range (C) | 1650-1800F |
| I.F.P. (celsius) | 650C |