Frit G-24

Description: LEADED FRIT

Oxide Analysis Formula Tolerance
CaO 4.65% 0.31
K2O 1.70% 0.07
Na2O 1.69% 0.10
PbO 31.64% 0.52
B2O3 13.02% 0.69
Al2O3 3.17% 0.12
SiO2 44.13% 2.72
Oxide Weight 370.39
Formula Weight 370.39

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3417
Materials Ferro Frit 3493
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.