Fusion Frit F-499

Alternate Names: Fusion Frit F499

Description: High sodium boron frit

Oxide Analysis Formula Tolerance
Na2O 21.00% 1.00
B2O3 28.40% 1.20
Al2O3 7.20% 0.21
SiO2 43.40% 2.13
Oxide Weight 295.24
Formula Weight 295.24

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3264
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.46 x 10-6
Frit Softening Point 1600F