Fusion Frit F-34

Alternate Names: Fusion Frit F34

Description: High boron zinc free calcium frit

Oxide Analysis Formula Tolerance
CaO 12.00% 0.51
Na2O 12.50% 0.49
B2O3 27.50% 0.95
SiO2 48.00% 1.92
Oxide Weight 240.66
Formula Weight 240.66

Related Information

Links

Materials Ferro Frit 3191
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3193
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.43 x 10-6
Frit Softening Point 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy