Fusion Frit F-215

Alternate Names: Frit F215

Oxide Analysis Formula Tolerance
CaO 6.21% 0.25
MgO 5.17% 0.29
Na2O 12.84% 0.46
B2O3 18.62% 0.60
Al2O3 8.62% 0.19
SiO2 48.54% 1.81
Oxide Weight 224.18
Formula Weight 224.18

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.