Alternate Names: Fusion Frit F105
Description: Alkali boron flux for wall tile
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 1.50% | 0.05 | |
| Na2O | 19.20% | 0.95 | |
| B2O3 | 21.00% | 0.93 | |
| Al2O3 | 6.80% | 0.20 | |
| SiO2 | 51.50% | 2.63 | |
| Oxide Weight | 307.12 | ||
| Formula Weight | 307.12 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 9.53 |
|---|---|
| Frit Softening Point | 1450F |
| By Tony Hansen Follow me on ![]() | ![]() |