Alternate Names: Frit P83, Frit 83
Description: Medium Lead Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 5.07% | 0.28 | |
| PbO | 46.96% | 0.72 | |
| B2O3 | 5.29% | 0.26 | |
| SiO2 | 42.68% | 2.43 | |
| Oxide Weight | 342.27 | ||
| Formula Weight | 342.27 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Frit HP33
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |