Alternate Names: Frit 4712
Description: Borosilicate hard clear general purpose frit 1040-1100C
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 9.55% | 0.60 | |
| K2O | 3.47% | 0.13 | |
| Na2O | 4.75% | 0.27 | |
| B2O3 | 12.44% | 0.63 | |
| Al2O3 | 10.13% | 0.35 | |
| SiO2 | 59.67% | 3.50 | |
| Oxide Weight | 352.54 | ||
| Formula Weight | 352.54 | ||
General purpose and versatile frit, good for strong and underglaze colors.
New name is Frit 4113.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 4113
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |