Ferro Frit 3516

Description: Lead calcium borosilicate frit

Oxide Analysis Formula Tolerance
CaO 12.30% 0.52
K2O 1.80% 0.05
Na2O 1.10% 0.04
PbO 37.60% 0.40
B2O3 13.00% 0.44
Al2O3 2.60% 0.06
SiO2 31.60% 1.24
Oxide Weight 235.54
Formula Weight 235.54

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 166
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.6
Frit Melting Range (C) 1400F