Ferro Frit 3465

Description: Low lead high borax frit cone 08-02

Oxide Analysis Formula Tolerance
CaO 6.50% 0.31
Na2O 14.40% 0.62
PbO 6.40% 0.08
B2O3 20.20% 0.77
SiO2 52.50% 2.32
Oxide Weight 265.40
Formula Weight 265.40

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit Pb-943
Materials Hommel Frit 18
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.70
Frit Melting Range (C) 1600F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy