Description: Leaded calcium boron free frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 6.91% | 0.35 | |
| Na2O | 0.65% | 0.03 | |
| PbO | 48.68% | 0.62 | |
| Al2O3 | 19.02% | 0.53 | |
| SiO2 | 24.74% | 1.17 | |
| Oxide Weight | 284.29 | ||
| Formula Weight | 284.29 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 402
|
| Materials |
Hommel Frit 555
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.6 |
|---|---|
| Frit Melting Range (C) | 1350F |