Description: Lead:silica 1:1 ratio frit (lead monosilicate)
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| PbO | 78.79% | 1.00 | |
| SiO2 | 21.21% | 1.00 | |
| Oxide Weight | 283.28 | ||
| Formula Weight | 283.28 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Frit A 1316
|
| Materials |
Lead Monosilicate Frit
A standard frit of 1 molar part of PbO and 1 of SiO2. It melts lower than a lead bisilicate. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |