Whitespar

Oxide Analysis Formula Tolerance
SiO2 66.00% 7.05 0.5
Al2O3 17.70% 1.11 0.5
Fe2O3 0.10% - Max
K2O 11.00% 0.75 Min
Na2O 2.10% 0.22 0.75
CaO 0.25% 0.03
MgO 0.03% -
LOI 0.30%n/a
Oxide Weight 623.57
Formula Weight 625.45

Notes

Intended for ceramics and glass.
K2O in minimum figure.
Fe2O3 is maximum figure.
LOI is maximum figure.

Available in 1200, 1250 and 1350 bulk bags and 25, 40 and 50 bags.
Available in 100, 200, 325 mesh sizes.

Related Information

WhiteSpar


This picture has its own page with more detail, click here to see it.

From India, Imerys Ceramics

Links


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy