Description: Leadless Alkaline Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 2.99% | 0.10 | |
| Na2O | 17.68% | 0.90 | |
| B2O3 | 20.73% | 0.94 | |
| Al2O3 | 6.79% | 0.21 | |
| SiO2 | 51.81% | 2.72 | |
| Oxide Weight | 315.55 | ||
| Formula Weight | 315.55 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |