Description: Ancienne fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 8.24% | 0.44 | |
| K2O | 3.97% | 0.13 | |
| Na2O | 9.11% | 0.44 | |
| Al2O3 | 7.25% | 0.21 | |
| B2O3 | 17.19% | 0.74 | |
| SiO2 | 54.25% | 2.69 | |
| Oxide Weight | 297.68 | ||
| Formula Weight | 297.68 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |