Chrome tin pink sphene stain

Formula: CaO:SnO:SiO2:Cr2O3

Notes

Chrome Tin Pink Sphene, an inorganic pigment, is a reaction product of high temperature calcination in which Calcium (II) Oxide, Tin (IV) Oxide, Silicon (IV)
Oxide, and Chromium (III) Oxide in varying amounts are homogeneously and ionically interdiffused to form a crystalline matrix of tin sphene.