Description: Leadless Borosilicate Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.40% | 0.56 | |
| K2O | 4.06% | 0.13 | |
| Na2O | 6.37% | 0.31 | |
| B2O3 | 28.58% | 1.24 | |
| Al2O3 | 9.80% | 0.29 | |
| SiO2 | 40.80% | 2.05 | |
| Oxide Weight | 301.94 | ||
| Formula Weight | 301.94 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |