Frit M-130

Description: Zircon frit

Oxide Analysis Formula Tolerance
CaO 3.84% 0.40
K2O 4.62% 0.29
Al2O3 8.75% 0.50
Na2O 2.28% 0.21
Li2O 0.51% 0.10
B2O3 18.77% 1.57
SiO2 51.86% 5.03
ZrO2 9.36% 0.44
Oxide Weight 583.43
Formula Weight 583.43

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.