Description: Barium zinc frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 35.63% | 0.50 | |
| ZnO | 18.92% | 0.50 | |
| Al2O3 | 5.22% | 0.11 | |
| SiO2 | 40.23% | 1.44 | |
| Oxide Weight | 215.12 | ||
| Formula Weight | 215.12 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Degussa Frit 90420
|