Alternate Names: Fusion Frit F498
Description: High magnesium flux
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 10.00% | 0.43 | |
| Na2O | 3.60% | 0.10 | |
| CaO | 15.50% | 0.47 | |
| Al2O3 | 10.50% | 0.18 | |
| B2O3 | 16.60% | 0.41 | |
| SiO2 | 43.80% | 1.25 | |
| Oxide Weight | 171.68 | ||
| Formula Weight | 171.68 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.92 x 10-6 |
|---|---|
| Frit Softening Point | 1500F |