Fusion Frit F-561

Alternate Names: Fusion Frit F561

Description: Barium-Zircon Matte frit

Oxide Analysis Formula Tolerance
Al2O3 5.00% 0.23
B2O3 11.50% 0.76
K2O 5.30% 0.26
BaO 24.60% 0.74
SiO2 46.00% 3.53
ZrO2 7.60% 0.28
Oxide Weight 461.40
Formula Weight 461.40

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.5 x 10-6
Frit Softening Point 1800F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy