Alternate Names: Frit 37 528, Frit 37-528
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.32% | 0.50 | |
| Na2O | 6.47% | 0.40 | |
| MgO | 0.53% | 0.05 | |
| ZnO | 1.06% | 0.05 | |
| B2O3 | 14.34% | 0.79 | |
| Al2O3 | 8.51% | 0.32 | |
| SiO2 | 61.77% | 3.94 | |
| Oxide Weight | 383.13 | ||
| Formula Weight | 383.13 | ||
| Frit Melting Range (C) | 940-1060C |
|---|