1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit 35.690

Alternate Names: Frit 35 690, Frit 35-690

Oxide Analysis Formula Tolerance
ZnO 1.24% 0.05
CaO 1.53% 0.09
BaO 12.12% 0.26
PbO 33.93% 0.50
K2O 2.00% 0.07
Na2O 0.57% 0.03
B2O3 1.06% 0.05
Al2O3 9.92% 0.32
SiO2 37.64% 2.06
Oxide Weight 328.97
Formula Weight 328.97

Related Information

Data

Frit Melting Range (C) 1020-1140C