Moulin Fritte M9152

Description: Fritte boro-calcique

Oxide Analysis Formula Tolerance
CaO 38.40% 1.00
B2O3 47.70% 1.00
Al2O3 7.70% 0.11
SiO2 6.20% 0.15
Oxide Weight 146.09
Formula Weight 146.09

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin

Data

Frit Softening Point 660C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy