Description: Very high alkali, zero boron, low alumina, high expansion frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.80% | 0.30 | |
| K2O | 13.00% | 0.30 | |
| Na2O | 11.40% | 0.40 | |
| Al2O3 | 1.40% | 0.03 | |
| SiO2 | 66.40% | 2.40 | |
| Oxide Weight | 216.96 | ||
| Formula Weight | 216.96 | ||
Commonly used to make crystalline glazes because of the very high alkali and very low alumina contents.
| Materials |
Mondre and Manz Frit 1233
|
| Materials |
Glasurfritten M1233
|
| Materials |
Degussa Frit 90208
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 503C |
|---|