Description: Fritte Raku
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 15.61% | 1.00 | |
| Al2O3 | 5.14% | 0.20 | |
| B2O3 | 26.29% | 1.50 | |
| SiO2 | 52.96% | 3.50 | |
| Oxide Weight | 397.18 | ||
| Formula Weight | 397.18 | ||
Corrected chemistry of this frit Oct 2022, it was:
BaO 26.3, Na2O 15.6, Al2O3 5.1, SiO2 53.0
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 565C |
|---|