Glasurfritten 37.06

Alternate Names: 37 06,37-06

Description: Bleifreie Barium-Fritte

Oxide Analysis Formula Tolerance
BaO 47.00% 1.00
Al2O3 17.00% 0.54
SiO2 36.00% 1.95
Oxide Weight 326.17
Formula Weight 326.17

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 70 x 10-7
Frit Melting Range (C) 1180-1280C