Glasurfritten 34.41

Alternate Names: 34 41,34-41

Description: Blei-Aluminium-Silikat-Fritte

Oxide Analysis Formula Tolerance
PbO 74.56% 1.00
Al2O3 4.78% 0.14
SiO2 20.66% 1.03
Oxide Weight 299.36
Formula Weight 299.36

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 77 x 10-7
Frit Softening Point 500C
Frit Melting Range (C) 900-1080C