1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Glasurfritten 33.17

Alternate Names: 33 17,33-17

Description: Bleifreie Zirkomfritte

Oxide Analysis Formula Tolerance
BaO 8.00% 0.11
K2O 3.00% 0.07
Na2O 14.00% 0.49
MgO 1.00% 0.05
ZnO 10.00% 0.27
Al2O3 16.00% 0.34
SiO2 48.00% 1.75
Oxide Weight 218.58
Formula Weight 218.58

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 90x10-7 603C
Frit Softening Point 603C
Frit Melting Range (C) 1000-1100C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy