Description: Fritte Alcaline
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 10.18% | 0.21 | |
| Na2O | 18.51% | 0.58 | |
| CaO | 3.03% | 0.10 | |
| BaO | 8.29% | 0.11 | |
| Al2O3 | 4.88% | 0.09 | |
| B2O3 | 3.76% | 0.10 | |
| SiO2 | 51.35% | 1.66 | |
| Oxide Weight | 194.29 | ||
| Formula Weight | 194.29 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Frit Melting Range (C) | 880-1060C |
|---|
| By Tony Hansen Follow me on ![]() | ![]() |