Hommel Frit 160

Description: Medium lead calcium borosilicate

Oxide Analysis Formula Tolerance
CaO 12.51% 0.51
Na2O 2.99% 0.11
PbO 37.24% 0.38
B2O3 13.25% 0.43
Al2O3 2.50% 0.06
SiO2 31.50% 1.20
Oxide Weight 228.25
Formula Weight 228.25

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.00
Co-efficient of Linear Expansion 8.0 x 10-6 (50-450C)
Frit Softening Point 1400F