Description: Reimbold & Strick fast fire high barium matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 5.00% | 0.09 | |
| K2O | 3.00% | 0.06 | |
| SiO2 | 34.00% | 1.07 | |
| ZnO | 21.00% | 0.49 | |
| BaO | 37.00% | 0.45 | |
| Oxide Weight | 188.26 | ||
| Formula Weight | 188.26 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 105 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | >800C |