Description: Reimbold & Strick high melting low exp matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 3.60% | 0.20 | |
| Al2O3 | 22.50% | 1.00 | |
| Li2O | 2.60% | 0.40 | |
| CaO | 5.00% | 0.40 | |
| SiO2 | 66.30% | 5.00 | |
| Oxide Weight | 453.31 | ||
| Formula Weight | 453.31 | ||
Until June 2021 the analysis shown here was approximate, this one is now more accurate.
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 18 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | >800C |