Description: Reimbold & Strick opacified stoneware opaque frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 7.00% | 0.32 | |
| CaO | 6.00% | 0.50 | |
| B2O3 | 13.00% | 0.87 | |
| ZrO2 | 12.00% | 0.45 | |
| K2O | 1.00% | 0.05 | |
| Na2O | 6.00% | 0.45 | |
| SiO2 | 55.00% | 4.27 | |
| Oxide Weight | 466.54 | ||
| Formula Weight | 466.54 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 58 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | 670C |
| Glass Transition Temperature | 600C |