Frit A 3360

Description: Reimbold & Strick barium stoneware frit

Oxide Analysis Formula Tolerance
Na2O 5.00% 0.28
Li2O 1.00% 0.12
CaO 7.00% 0.44
SiO2 58.00% 3.39
B2O3 15.00% 0.76
BaO 7.00% 0.16
Al2O3 7.00% 0.24
Oxide Weight 351.32
Formula Weight 351.32

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 60 x 10-7 (20-400C)
Frit Softening Point 650C
Glass Transition Temperature 590C