| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 0.35% | 0.10 | |
| CaO | 0.24% | 0.05 | |
| Na2O | 4.52% | 0.85 | |
| Al2O3 | 7.88% | 0.90 | |
| SiO2 | 65.51% | 12.69 | |
| B2O3 | 21.50% | 3.60 | |
| Oxide Weight | 1,164.60 | ||
| Formula Weight | 1,164.60 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 48 X 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 495C |
| Heating Microscope Analysis for Frits | 795C |
| Heating Microscope Analysis for Frits | 1270C |