Alternate Names: 90016 Alkaliborfritte
Description: Alkaibortntte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.37% | 0.50 | |
| B2O3 | 9.15% | 0.50 | |
| Na2O | 4.07% | 0.25 | |
| K2O | 6.19% | 0.25 | |
| Al2O3 | 6.70% | 0.25 | |
| SiO2 | 45.81% | 2.90 | |
| Oxide Weight | 301.79 | ||
| Formula Weight | 301.79 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 76 x 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 564C |
| Heating Microscope Analysis for Frits | 790C |
| Heating Microscope Analysis for Frits | 960C |