Ground Magnetite

Formula: Fe3O4

Oxide Analysis Formula Tolerance
Fe2O3 66.17% 1.00
FeO 33.83% 1.00
Oxide Weight 241.80
Formula Weight 241.80

Notes

Natural Magnetite is most commonly used in the coal industry. Like raw hematite, it can contain 5-15% impurities. However the price of synthetic black iron oxide can be 500% more than the finely ground raw material. Thus most companies will use the cheaper ground natural magnetite where possible.

Related Information

Links

Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Minerals Magnetite
A black, hard, dense and stable crystalline mineral form of iron oxide.
Materials Hematite
Materials Iron Oxide Black

Data

Frit Softening Point 1538C D

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy