March 2026: We are doing major upgrades to code here, please be patient regarding any issues. If any page is not working for a period of hours, please contact us. Thank you.
| Monthly Tech-Tip | No tracking! No ads! No paywall! |
Alternate Names: Fritte C1253, Fritte C 1253, Ceradel Frit 1253
Description: High expansion frit, Fritte boro-alcaline sans plomb
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 2.54% | 0.05 | 10 |
| B2O3 | 21.72% | 0.95 | 10 |
| Al2O3 | 6.43% | 0.19 | 15 |
| Na2O | 13.37% | 0.66 | 3 |
| CaO | 3.91% | 0.21 | .5 |
| ZnO | 2.16% | 0.08 | |
| SiO2 | 49.86% | 2.53 | |
| Oxide Weight | 304.43 | ||
| Formula Weight | 304.43 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Co-efficient of Linear Expansion | 99x10-7 (20/300C) |
|---|---|
| Frit Softening Point | 880-920C |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk