Description: Cuban silica
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 1.03% | 0.49 | |
| MgO | 0.30% | 0.36 | |
| CaO | 0.75% | 0.64 | |
| SiO2 | 97.00% | 77.55 | |
| Fe2O3 | 0.70% | 0.21 | |
| 0.23% | - | ||
| LOI | 0.48% | n/a | |
| Oxide Weight | 4,794.08 | ||
| Formula Weight | 4,817.21 | ||
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |
| Materials |
Silica Sierra Cristal (Cuba)
|