Description: Cuban silica
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 1.93% | 0.48 | |
| MgO | 0.16% | 0.10 | |
| CaO | 2.00% | 0.90 | |
| SiO2 | 95.48% | 40.10 | |
| Fe2O3 | 0.76% | 0.12 | |
| LOI | 0.23% | n/a | |
| Oxide Weight | 2,532.25 | ||
| Formula Weight | 2,538.09 | ||
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |
| Materials |
Silica Sierra Cristal (Cuba)
|