Description: Uganda ball clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 0.23% | 0.02 | |
| Al2O3 | 23.42% | 1.00 | |
| Na2O | 0.13% | 0.01 | |
| SiO2 | 54.78% | 3.97 | |
| P2O5 | 0.14% | - | |
| K2O | 1.02% | 0.05 | |
| CaO | 0.46% | 0.04 | |
| TiO2 | 1.83% | 0.10 | |
| Fe2O3 | 7.33% | 0.20 | |
| Cr2O3 | 0.02% | - | |
| MnO | 0.03% | - | |
| CuO | 0.02% | - | |
| ZrO2 | 0.10% | - | |
| LOI | 10.02% | n/a | |
| SO3 | 0.29% | n/a | |
| Oxide Weight | 389.84 | ||
| Formula Weight | 434.65 | ||
Analysis from SEAMIC labs in 2007.
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |