Ceradel Frit C 1251

Alternate Names: C1251 Fritte, C 1251 Fritte, Ceradel Frit 1251

Description: Lead monosilicate frit, Monosilicate de plomb

Oxide Analysis Formula Tolerance
SiO2 21.21% 1.00
PbO 78.79% 1.00
Oxide Weight 283.28
Formula Weight 283.28

Notes

This analysis is guessed, the manufacturer calls it a lead monosilicate and provides the approximate chemistry of (SiO2 - 15-40%, PbO 60-100%). However, since the lead monosilicate analysis is theoretically 1:1 lead:silica that is what we have assigned here.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ceradel Frit C 1249
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.
Materials Lead Monosilicate Frit
A standard frit of 1 molar part of PbO and 1 of SiO2. It melts lower than a lead bisilicate.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.

Data

Co-efficient of Linear Expansion 83x10-7 (20-300C)
Frit Softening Point 900-1100C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy