| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 77.00% | 10.98 | |
| Fe2O3 | 1.57% | 0.08 | |
| Al2O3 | 11.90% | 1.00 | |
| TiO2 | 2.26% | 0.24 | |
| MgO | 0.27% | 0.06 | |
| K2O | 0.57% | 0.05 | |
| CaO | 0.32% | 0.05 | |
| Na2O | 0.09% | 0.01 | |
| P2O5 | 0.04% | - | |
| SO4 | 5.50% | n/a | |
| Oxide Weight | 805.89 | ||
| Formula Weight | 852.79 | ||
| Materials |
Fireclay
|
| Typecodes |
Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service. |
| Typecodes |
Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more. |