Description: Soft sodium borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 5301
|
| Materials |
Ferro Frit 4125
|
| Materials |
Ferro Frit 4194
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |