Kaolin G1

Oxide Analysis Formula Tolerance
CaO 0.13% 0.01
K2O 2.62% 0.13
Na2O 0.40% 0.03
TiO2 0.73% 0.04
Al2O3 22.50% 1.00
SiO2 67.30% 5.08
Fe2O3 0.32% 0.01
LOI 6.00%n/a
Oxide Weight 426.13
Formula Weight 453.33

Related Information

Links

Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy