1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Silver Chloride

Formula: AgCl

Oxide Analysis Formula Tolerance
Ag2O 80.82% 1.00
Cl 24.75%n/a
Oxide Weight 231.74
Formula Weight 307.95

Related Information

Links

Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Materials Silver Nitrate
URLs http://en.wikipedia.org/wiki/Silver_chloride