Frit Welte FR 2020

Description: Lead bisilicate monoborate frit

Formula: PbO.B2O3.2SiO2

Oxide Analysis Formula Tolerance
B2O3 16.85% 1.00
PbO 54.04% 1.00
SiO2 29.10% 2.00
Oxide Weight 412.99
Formula Weight 412.99

Related Information

Links

Typecodes Leaded Frit