Frit Welte FR 2015

Description: Lead bisilicate frit

Formula: PbO.2SiO2

Oxide Analysis Formula Tolerance
PbO 60.02% 1.00
Al2O3 6.86% 0.25
SiO2 33.13% 2.05
Oxide Weight 371.91
Formula Weight 371.91

Related Information

Links

Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Lead Bisilicate Frit
A standard frit of 1 molar part of PbO and 2 of SiO2. It is considered stable and non-leachable.

Data

Co-efficient of Linear Expansion 52.2 x10-7 (20-400C)
Glass Transition Temperature 565C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy